• Laser & Optoelectronics Progress
  • Vol. 57, Issue 3, 031402 (2020)
Peng Liu1, Zhikai Chen2、3、*, Quanming Jin1, and Qinghai Zhu2、3
Author Affiliations
  • 1Xuzhou Construction Machinery Group Hydraulics Business Division, Xuzhou, Jiangsu 221004, China
  • 2Jiangsu Xuzhou Construction Machinery Research Institute Co., Ltd., Xuzhou, Jiangsu 221004, China
  • 3State Key Laboratory of Intelligent Manufacturing of Advanced Construction Machinery, Xuzhou, Jiangsu 221004, China
  • show less
    DOI: 10.3788/LOP57.031402 Cite this Article Set citation alerts
    Peng Liu, Zhikai Chen, Quanming Jin, Qinghai Zhu. Microstructure and Corrosion Behaviors of 316L Coating Fabricated by Laser Cladding[J]. Laser & Optoelectronics Progress, 2020, 57(3): 031402 Copy Citation Text show less
    References

    [1] Moustafa S F, Abdel-Hamid Z, Baheig O G et al. Synthesis of WC hard materials using coated powders[J]. Advanced Powder Technology, 22, 596-601(2011).

    [2] Lang F Q, Yu Z M. The corrosion resistance and wear resistance of thick TiN coatings deposited by arc ion plating[J]. Surface and Coatings Technology, 145, 80-87(2001).

    [3] Tuominen J, Vuoristo P, Mäntylä T et al. Corrosion behavior of HVOF-sprayed and Nd-YAG laser-remelted high-chromium, nickel-chromium coatings[J]. Journal of Thermal Spray Technology, 11, 233-243(2002).

    [4] Shi L, Sun C F, Gao P et al. Mechanical properties and wear and corrosion resistance of electrodeposited Ni-Co/SiC nanocomposite coating[J]. Applied Surface Science, 252, 3591-3599(2006).

    [5] Huang C A, Chuang C H, Lin C K. Wear and corrosion resistance of Cr-C deposits obtained from a trivalent chromium electroplating bath with the addition of nanosized Al2O3 powder[J]. Trends in Neurosciences, 14, 389-90(2012).

    [6] Berger L M, Lipp K, Spatzier J et al. Dependence of the rolling contact fatigue of HVOF-sprayed WC-17%Co hardmetal coatings on substrate hardness[J]. Wear, 271, 2080-2088(2011).

    [7] Wang Q Y, Zhang Y F, Bai S L et al. Microstructures, mechanical properties and corrosion resistance of Hastelloy C22 coating produced by laser cladding[J]. Journal of Alloys and Compounds, 553, 253-258(2013).

    [8] Dehm G, Bamberger M. Laser cladding of Co-based hardfacing on Cu substrate[J]. Journal of Materials Science, 37, 5345-5353(2002).

    [9] Farahmand P, Kovacevic R. Corrosion and wear behavior of laser cladded Ni-WC coatings[J]. Surface and Coatings Technology, 276, 121-135(2015).

    [10] Wang H M, Wang C M, Cai L X. Wear and corrosion resistance of laser clad Ni2Si/NiSi composite coatings[J]. Surface and Coatings Technology, 168, 202-208(2003).

    [11] Sun L L, Zhu C, Wang Y et al. Carbon dioxide corrosion behavior of Fe-based high chromium laser cladding coating[J]. Ordnance Material Science and Engineering, 35, 22-26(2012).

    [12] Wu W H, Yang Y Q, Wang D. Balling phenomenon in selective laser melting process[J]. Journal of South China University of Technology(Natural Science Edition), 38, 110-115(2010).

    [13] Kain V, Chandra K, Adhe K N et al. Effect of cold work on low-temperature sensitization behaviour of austenitic stainless steels[J]. Journal of Nuclear Materials, 334, 115-132(2004).

    Peng Liu, Zhikai Chen, Quanming Jin, Qinghai Zhu. Microstructure and Corrosion Behaviors of 316L Coating Fabricated by Laser Cladding[J]. Laser & Optoelectronics Progress, 2020, 57(3): 031402
    Download Citation