[3] BOCHENEK A, BOBER B, HAUFFE W, et al. Thermal degradation of joined thick Au and Al elements [J]. Microelec Int, 2004, 21(1): 31-34.
[4] ZHONG Z W. Wire bonding using insulated wire and new challenges in wire bonding [J]. Microelec Int, 2008, 25(2): 9-14.
[8] LIU Y X, CHEN Y T, GU S, et al. Fracture reliability concern of (Au, Ni)Sn 4 phase in 3D integrated circuit microbumps using Ni/Au surface finishing [J]. Scripta Materialia, 2016, 119(119): 9-12.