• Chinese Optics Letters
  • Vol. 19, Issue 4, 041402 (2021)
Chao Tan1, Linjie Zhao1, Mingjun Chen1、*, Jian Cheng1、**, Zhaoyang Yin1, Qi Liu1, Hao Yang1, and Wei Liao2
Author Affiliations
  • 1State Key Laboratory of Robotics and System, Harbin Institute of Technology, Harbin 150001, China
  • 2Research Center of Laser Fusion, China Academy of Engineering Physics, Mianyang 621900, China
  • show less
    DOI: 10.3788/COL202119.041402 Cite this Article Set citation alerts
    Chao Tan, Linjie Zhao, Mingjun Chen, Jian Cheng, Zhaoyang Yin, Qi Liu, Hao Yang, Wei Liao. Combined studies of surface evolution and crack healing for the suppression of negative factors during CO2 laser repairing of fused silica[J]. Chinese Optics Letters, 2021, 19(4): 041402 Copy Citation Text show less

    Abstract

    In order to reveal the evolution mechanism of repaired morphology and the material’s migration mechanism on the crack surface in the process of CO2 laser repairing surface damage of fused silica optics, two multi-physics coupling mathematical models with different scales are developed, respectively. The physical problems, such as heat and mass transfer, material phase transition, melt flow, evaporation removal, and crack healing, are analyzed. Studies show that material ablation and the gasification recoil pressure accompanying the material splash are the leading factors in forming the Gaussian crater with a raised rim feature. The use of low-power lasers for a long time can fully melt the material around the crack before healing, which can greatly reduce the size of the residual air layer. Combined with the experimental research, the methods to suppress the negative factors (e.g., raised rim, deposited debris, air bubbles) in the CO2 laser repairing process are proposed.
    ρu=0,

    View in Article

    ρCpTt+ρCp(u·T)=·(kT),

    View in Article

    ρut+ρ(u·)u=·[pA+μ(u)+(u)T]ρ[1β(TTm)]g+F,

    View in Article

    σ=σ0γ(TTm),

    View in Article

    σn=κσ·n,

    View in Article

    σt=σTsT·t,

    View in Article

    qevap=Mv×Lv,

    View in Article

    Mv=m2πkbT×Psat(T)×(1βr),

    View in Article

    Psat(T)=Patm×exp[MaLvR(1Tv1T)],

    View in Article

    Precoil={Patm,0Ts<Tv1+βr2×Psat(Ts),TsTv.

    View in Article

    τ=ηw/(πσ),

    View in Article

    d=2πkTsEa,

    View in Article

    Chao Tan, Linjie Zhao, Mingjun Chen, Jian Cheng, Zhaoyang Yin, Qi Liu, Hao Yang, Wei Liao. Combined studies of surface evolution and crack healing for the suppression of negative factors during CO2 laser repairing of fused silica[J]. Chinese Optics Letters, 2021, 19(4): 041402