• Laser & Optoelectronics Progress
  • Vol. 55, Issue 11, 111401 (2018)
Yanan Liu1、*, Ronglu Sun1、2、**, Tiangang Zhang3, and Meijia Li1
Author Affiliations
  • 1 School of Mechanical Engineering, Tianjin Polytechnic University, Tianjin 300387, China
  • 2 Tianjin Key Laboratory of Advanced Mechatronics Equipment Technology, Tianjin Polytechnic University, Tianjin 300387, China
  • 3 Engineering Technology Training Center, Civil Aviation University of China, Tianjin 300300, China
  • show less
    DOI: 10.3788/LOP55.111401 Cite this Article Set citation alerts
    Yanan Liu, Ronglu Sun, Tiangang Zhang, Meijia Li. Effect of CeO2 Content on Microstructure and Properties of Laser Cladded Self-Lubricant Coatings[J]. Laser & Optoelectronics Progress, 2018, 55(11): 111401 Copy Citation Text show less
    Surface morphologies of coatings with different CeO2 contents. (a) Single-pass laser cladding; (b) multi-track laser lap cladding
    Fig. 1. Surface morphologies of coatings with different CeO2 contents. (a) Single-pass laser cladding; (b) multi-track laser lap cladding
    XRD patterns of coatings with different CeO2 contents
    Fig. 2. XRD patterns of coatings with different CeO2 contents
    SEM images in middle parts of coatings with different CeO2 contents. (a) 0; (b) 0.5%; (c) 1.0%; (d) 1.5%; (e) 2.0%
    Fig. 3. SEM images in middle parts of coatings with different CeO2 contents. (a) 0; (b) 0.5%; (c) 1.0%; (d) 1.5%; (e) 2.0%
    EDS analysis of phases for coatings. (a) A1; (b) A2; (c) A3; (d) A4; (e) A5
    Fig. 4. EDS analysis of phases for coatings. (a) A1; (b) A2; (c) A3; (d) A4; (e) A5
    Structural morphologies in middle-upper part of coatings
    Fig. 5. Structural morphologies in middle-upper part of coatings
    Cross-sectional micro-hardness distribution of coatings with different CeO2 contents
    Fig. 6. Cross-sectional micro-hardness distribution of coatings with different CeO2 contents
    Wear surface morphologies of coatings with different CeO2 contents. (a) 0; (b) 0.5%; (c) 1.0%; (d) 1.5%; (e) 2.0%
    Fig. 7. Wear surface morphologies of coatings with different CeO2 contents. (a) 0; (b) 0.5%; (c) 1.0%; (d) 1.5%; (e) 2.0%
    Friction coefficients of coatings with different CeO2 contents
    Fig. 8. Friction coefficients of coatings with different CeO2 contents
    Wear mass losses of coatings with different CeO2 contents
    Fig. 9. Wear mass losses of coatings with different CeO2 contents
    MaterialMass fraction /%Melting point /℃Size /μmLinear expansioncoefficient /(10-6 K)
    TC46.01(Al),3.8(V),0.1(C),0.3(Fe),Bal.(Ti)1660-9.6
    Ni6016(Cr),3.5(B),4.5(Si),0.8(C),≤15(Fe),Bal.(Ni)960-104050-10013.4
    Ti3SiC230002-49.2
    CeO2239720-40-
    Table 1. Chemical compositions and physical parameters of original materials
    PhaseContentBCAlSiTiVCrFeNi
    A1Mass fraction /%-15.18--81.73-0.930.461.70
    Atom fraction /%-41.78--56.40-0.590.270.96
    A2Mass fraction /%29.486.640.340.8554.481.512.501.262.93
    Atom fraction /%59.1511.990.280.6624.670.641.040.491.08
    A3Mass fraction /%-2.812.246.5939.452.5711.119.2126.02
    Atom fraction /%-10.423.7010.4436.642.249.517.3419.72
    A4Mass fraction /%-2.774.221.8136.930.945.136.4841.82
    Atom fraction /%-10.647.222.9835.500.854.565.3632.89
    A5Mass fraction /%-6.812.406.6238.242.7710.447.6725.06
    Atomfraction /%-22.593.549.4031.812.168.005.4817.01
    Table 2. EDS analysis results of coatings
    Yanan Liu, Ronglu Sun, Tiangang Zhang, Meijia Li. Effect of CeO2 Content on Microstructure and Properties of Laser Cladded Self-Lubricant Coatings[J]. Laser & Optoelectronics Progress, 2018, 55(11): 111401
    Download Citation