• Journal of Inorganic Materials
  • Vol. 36, Issue 10, 1111 (2021)
Longbin LI1、2, Yudong XUE1、2, Jianbao HU1、2, Jinshan YANG1、2, Xiangyu ZHANG1、2, and Shaoming DONG1、2、*
Author Affiliations
  • 11. State Key Laboratory of High Performance Ceramics and Superfine Microstructure, Shanghai Institute of Ceramics, Chinese Academy of Sciences, Shanghai 200050, China
  • 22. Center of Materials Science and Optoelectronics Engineering, University of Chinese Academy of Sciences, Beijing 100049, China
  • show less
    DOI: 10.15541/jim20210045 Cite this Article
    Longbin LI, Yudong XUE, Jianbao HU, Jinshan YANG, Xiangyu ZHANG, Shaoming DONG. Influence of SiC Nanowires on the Damage Evolution of SiCf/SiC Composites [J]. Journal of Inorganic Materials, 2021, 36(10): 1111 Copy Citation Text show less
    References

    [1] R NASLAIN. Design, preparation and properties of non-oxide CMCs for application in engines and nuclear reactors: an overview. Composites Science and Technology, 64, 155-170(2004).

    [2] A DICARLO J, M van ROODE. Ceramic Composite Development for Gas Turbine Engine Hot Section Components. Barcelona, Spain, 221-231(2006).

    [3] R NASLAIN R. Processing of non-oxide ceramic matrix composites: an overview. Advances in Science and Technology, 50, 64-74(2006).

    [4] X YIN, L CHENG, L ZHANG et al. Fibre-reinforced multifunctional SiC matrix composite materials. International Materials Reviews, 62, 117-172(2017).

    [5] W YANG, H ARAKI, C TANG et al. Single-crystal SiC nanowires with a thin carbon coating for stronger and tougher ceramic composites. Advanced Materials, 17, 1519-1523(2005).

    [6] J HU, S DONG, Q FENG et al. Tailoring carbon nanotube/matrix interface to optimize mechanical properties of multiscale composites. Carbon, 69, 621-625(2014).

    [7] G ZHU, Y XUE, J HU et al. Influence of boron nitride nanotubes on the damage evolution of SiCf/SiC composites. Journal of the European Ceramic Society, 38, 4614-4622(2018).

    [8] F HE, Y LIU, Z TIAN et al. Carbon fiber/SiC composites modified SiC nanowires with improved strength and toughness. Materials Science and Engineering: A, 734, 374-384(2018).

    [9] Y CHU, H LI, Q FU et al. Oxidation protection and behavior of C/C composites with an in situ SiC nanowire-SiC-Si/SiC-Si coating. Corrosion Science, 70, 285-289(2013).

    [10] K ZHAO, K LI, Y WANG. Rapid densification of C/SiC composite by incorporating SiC nanowires. Composites Part B: Engineering, 45, 1583-1586(2013).

    [11] R DONG, W YANG, P WU et al. Effect of reinforcement shape on the stress-strain behavior of aluminum reinforced with SiC nanowire. Materials & Design, 88, 1015-1020(2015).

    [12] D THOULESS M, G EVANS A. Effects of pull-out on the mechanical properties of ceramic-matrix composites. Acta Metallurgica, 36, 517-522(1988).

    [13] N DE GREEF, L GORBATIKH, A GODARA et al. The effect of carbon nanotubes on the damage development in carbon fiber/epoxy composites. Carbon, 49, 4650-4664(2011).

    [14] M KANG S, J KIM W, G YOON S et al. Effects of the PyC interface coating on SiC nanowires of SiCf/SiC composite. Journal of Nuclear Materials, 417, 367-370(2011).

    [15] N MORSCHER G, M SINGH, D KISER J et al. Modeling stress-dependent matrix cracking and stress-strain behavior in 2D woven SiC fiber reinforced CVI SiC composites. Composites Science and Technology, 67, 1009-1017(2007).

    [16] T WHITLOW, E JONES, C PRZYBYLA. In-sit damage monitoring of a SiC/SiC ceramic matrix composite using acoustic emission and digital image correlation. Composite Structures, 158, 245-251(2016).

    [17] N MORSCHER G. Stress-dependent matrix cracking in 2D woven SiC-fiber reinforced melt-infiltrated SiC matrix composites. Composites Science and Technology, 64, 1311-1319(2004).

    [18] S ARGON A. Fracture of composites. Treatise on Materials Science and Technology, 1, 79-114(1972).

    Longbin LI, Yudong XUE, Jianbao HU, Jinshan YANG, Xiangyu ZHANG, Shaoming DONG. Influence of SiC Nanowires on the Damage Evolution of SiCf/SiC Composites [J]. Journal of Inorganic Materials, 2021, 36(10): 1111
    Download Citation