[1] Pritula L, Gayvoronsky V, et al. Effect of incorporation of titanium dioxide nanocrystals on bulk properties of KDP crystals [J]. Optical Materials, 2011, 33(4): 623-630.
[2] Ding J X, Wang S L, et al. AFM investigation on step bunching on (100) face of KDP crystal [J]. Journal of Inorganic Materials, 2010, 25(11): 1191-1194.
[3] Wang Xiaoding, Li Mingwei, et al. Computational analysis of three-dimensional flow and mass transfer in a non-standard configuration for growth of a KDP crystal [J]. Journal of Crystal Growth, 2010, 312(20): 2952-2961.
[4] Yakushkin E D, Efremova E P. Growth conditions and electrical properties of KDP crystals: II. dielectric permittivity measurements [J]. Physical Properties of Crytals, 2010, 55(1): 109-113.
[7] Zaitseva N, Atherton J, et al. Design and benefits of continuous filtration in rapid growth of large KDP and DKDP crystal [J]. Journal of Crystal Growth, 1999, 197: 911.
[8] Zaitseva N, Garman L. Rapid growth of KDP-type crystal [J]. Progress in Crystal Growth and Characterization of Materials, 2001, 43: 27-28.
[9] Srinivasan K, Meera K, Rammasamy P. A contemporary method to enhance the metastable zone width for crystal growth from solution [J]. Materials Science and Engineering, 2001, 84: 233-236.
[10] Podder J. The study of impurities effect on the growth and nucleation kinetics of potassium dihydrogen phosphate [J]. Journal of Crystal Growth, 2002, 237: 70-75.
[13] Kim K M, Temple H E. Growth of optically homogeneous single crystals of Pb5 GeO4 (VO4 )2 from the melt [J]. Journal of Crystal Growth, 1976, 34(2): 177-180.