  • Vol. 56, Issue 2, 021602 (2019)
Gaosong Li, Jinhua Li*, Pengchao Shan, and Weilong Feng
Author Affiliations
  • College of Mechanical Engineering and Automation, Liaoning University of Technology, Jinzhou, Liaoning 121001, China
  • show less
    DOI: 10.3788/LOP56.021602 Cite this Article Set citation alerts
    Gaosong Li, Jinhua Li, Pengchao Shan, Weilong Feng. Effect of WC-Reinforced Ni60AA on Cracks and Hardness[J]. Laser & Optoelectronics Progress, 2019, 56(2): 021602 Copy Citation Text show less
    Macroscopic morphologies under different powder feeding voltage ratios. (a) 3∶2; (b) 1∶1; (c) 2∶3
    Fig. 1. Macroscopic morphologies under different powder feeding voltage ratios. (a) 3∶2; (b) 1∶1; (c) 2∶3
    Macroscopic morphologies under different specific powders and specific energies. (a) Specific energy of 140, specific powder of 12; (b) specific energy of 200, specific powder of 12; (c) specific energy of 100, specific powder of 9
    Fig. 2. Macroscopic morphologies under different specific powders and specific energies. (a) Specific energy of 140, specific powder of 12; (b) specific energy of 200, specific powder of 12; (c) specific energy of 100, specific powder of 9
    Laser cladding process
    Fig. 3. Laser cladding process
    Morphologies under different vibration frequencies. (a) 0 Hz; (b) 22000 Hz; (c) 28000 Hz
    Fig. 4. Morphologies under different vibration frequencies. (a) 0 Hz; (b) 22000 Hz; (c) 28000 Hz
    Microhardness change from top to bottom of cladding layer
    Fig. 5. Microhardness change from top to bottom of cladding layer
    Morphologies under different powder feeding voltage ratios. (a) 1∶4; (b) 3∶7; (c) 2∶3; (d) 3∶2
    Fig. 6. Morphologies under different powder feeding voltage ratios. (a) 1∶4; (b) 3∶7; (c) 2∶3; (d) 3∶2
    MaterialCCrSiBFeNiWCCo
    Ni60AA0.4-0.913-173.2-4.82.5-4.0≤8.0margin00
    WC000000margin8.0
    Table 1. Mass fractions for components of Ni60AA and WC%
    Serial numberPowder feedingvoltage ratioTotal powderfeeding voltage /VLaser power /WScanningspeed /(m·s-1)
    a3∶2247002
    b1∶1247002
    c2∶3247002
    Table 2. Laser processing parameters
    Specific powder24681012
    Increase of cladding layer0.150.270.540.610.700.89
    Melting depth of substrate1.040.890.760.680.550.37
    Maximum microhardness410730790812835839
    Table 3. Influence of specific powder on increase of cladding layer and maximum microhardness
    Gaosong Li, Jinhua Li, Pengchao Shan, Weilong Feng. Effect of WC-Reinforced Ni60AA on Cracks and Hardness[J]. Laser & Optoelectronics Progress, 2019, 56(2): 021602