[1] Yang Guang, Wang Xiangming, Wang Wei, et al. Microstructure and property of laser cladding TiC reinforced composition coating[J]. Infrared and Laser Engineering, 2014, 43(3): 795-799. (in Chinese)
[2] Tang Shujun, Liu Hongxi, Zhang Xiaowei, et al.Microstructure and property of selective laser cladding Ni-Al intermetallic compound coating on H13 steel surface[J]. Infrared and Laser Engineering, 2014, 43(5): 1621-1626. (in Chinese)
[3] An Xulong, Liu Qibin, Zheng Bo. Microstructure and properties of laser cladding high entropy alloy MoFeCrTiWAl_xSi_y coating[J]. Infrared and Laser Engineering, 2014, 43(4): 1140-1144. (in Chinese)
[5] Yu Lingling, Shi Shihong, Di Keyun. Research on the laser cladding inclined wall accumulation based on the internal laser coaxial-powderFeeding technology[J]. Laser and Infrared, 2009, 39(3): 264-266. (in Chinese)
[8] Cai Wei, Fu Geyan, Shi Shihong, et al. Research on thickness control of variable diameter solid with coaxial inside-beam powder feeding laser cladding by defocusing technique[J]. Chinese J Lasers, 2012, 39(7): 0703003. (in Chinese)
[10] Fu Geyan, Liu Yu, Shi Shihong, et al. Control of process parameters for accumulate screwy thin-walled part by laser cladding with coaxial inside-beam powder feeding[J],Electromachining and Mould, 2014(2): 43-46. (in Chinese)