• Laser & Optoelectronics Progress
  • Vol. 56, Issue 18, 181402 (2019)
Tongtong Li1、2, Baodong Shen2、3、*, Chonghe Li1、2, Baobao Lan1、2, and Guangyao Chen2
Author Affiliations
  • 1 State Key Laboratory of Advanced Special Steel, Shanghai University, Shanghai 200072, China
  • 2 School of Materials Science and Engineering, Shanghai University, Shanghai 200072, China
  • 3 Shanghai Yinma Marking Co., Ltd., Shanghai 201601, China
  • show less
    DOI: 10.3788/LOP56.181402 Cite this Article Set citation alerts
    Tongtong Li, Baodong Shen, Chonghe Li, Baobao Lan, Guangyao Chen. Laser Surface Processing on Anodic Aluminum Oxide[J]. Laser & Optoelectronics Progress, 2019, 56(18): 181402 Copy Citation Text show less
    Working schematic of laser marking equipment
    Fig. 1. Working schematic of laser marking equipment
    Macroscopic displays on surface of 5052 anodic aluminum oxide alloy after laser surface processing with different setup powers. (a) 23%P0; (b) 25%P0; (c) 27%P0; (d) 33%P0; (e) 38%P0; (f) 40%P0; (g) 50%P0
    Fig. 2. Macroscopic displays on surface of 5052 anodic aluminum oxide alloy after laser surface processing with different setup powers. (a) 23%P0; (b) 25%P0; (c) 27%P0; (d) 33%P0; (e) 38%P0; (f) 40%P0; (g) 50%P0
    Laser output power as a function of pattern contrast
    Fig. 3. Laser output power as a function of pattern contrast
    Micro-morphologies on surface of 5052 anodic aluminum oxide alloy after laser surface processing with different setup powers. (a) 1.64 W; (b) 1.88 W; (c) 2.13 W; (d) 2.76 W; (e) 3.32 W; (f) 3.58 W; (g) 4.66 W
    Fig. 4. Micro-morphologies on surface of 5052 anodic aluminum oxide alloy after laser surface processing with different setup powers. (a) 1.64 W; (b) 1.88 W; (c) 2.13 W; (d) 2.76 W; (e) 3.32 W; (f) 3.58 W; (g) 4.66 W
    SEM micro-morphologies of aluminum surface before and after laser surface processing. (a) 500×; (b) local amplification for 5000×
    Fig. 5. SEM micro-morphologies of aluminum surface before and after laser surface processing. (a) 500×; (b) local amplification for 5000×
    SEM micro-morphologies of aluminum cross section. (a) Before laser surface processing; (b) after laser surface processing
    Fig. 6. SEM micro-morphologies of aluminum cross section. (a) Before laser surface processing; (b) after laser surface processing
    SEM micro-morphologies of aluminum surface before and after laser surface processing with setup power of 38%P0
    Fig. 7. SEM micro-morphologies of aluminum surface before and after laser surface processing with setup power of 38%P0
    CompositionAlMgFeSiCrCuMnZn
    ContentBal.2.2-2.80.250.250.15-0.350.10.10.1
    Table 1. Chemical compositions of 5052 aluminum alloy (mass fraction, %)
    ParameterValue
    Scanning speed /(mm·s-1)130
    Setup power /P023%,25%,27%,33%,38%,40%,50%
    Frequency/ kHz300
    Pulse length/ns4
    Scanning distance/mm0.005
    Table 2. Parameters of laser surface processing
    Tongtong Li, Baodong Shen, Chonghe Li, Baobao Lan, Guangyao Chen. Laser Surface Processing on Anodic Aluminum Oxide[J]. Laser & Optoelectronics Progress, 2019, 56(18): 181402
    Download Citation