• Journal of Infrared and Millimeter Waves
  • Vol. 40, Issue 2, 166 (2021)
Yi LIU, Ji-Qing JIAO*, Bai-Ze LYU, and Jiu-Xing WANG
Author Affiliations
  • College of Materials Science and Engineering, National Center of International Joint Research for Hybrid Materials Technology, National Base of International Sci. & Tech. Cooperation, Qingdao University, Qingdao 266071, China
  • show less
    DOI: 10.11972/j.issn.1001-9014.2021.02.005 Cite this Article
    Yi LIU, Ji-Qing JIAO, Bai-Ze LYU, Jiu-Xing WANG. The heterostructure NaGdF4:Yb,Er nanorods loaded on metal-organic frameworks for tuning upconversion photoluminescence[J]. Journal of Infrared and Millimeter Waves, 2021, 40(2): 166 Copy Citation Text show less

    Abstract

    Multi-component heterostructure nanocomposites can not only inherit the original properties of each component, but also induce new chemical and electronic properties through the interaction between the components. The heterostructure zeolitic imidazolate framework/NaGdF4:Yb,Er (ZIF-67/NaGdF4:Yb,Er) was prepared by a stepwise synthesis strategy. And it avoided agglomeration and quenching of upconversion (UC) nanoparticles, and displayed better stability. In the heterostructure nanocomposites, ZIF-67 is employed as an energy transmission platform under 980 nm excitation. Compared to pure NaGdF4:Yb,Er nanorods, the UC photoluminescence of heterostructure ZIF-67/NaGdF4:Yb,Er is tuned from green to red owing to the synergistic effect of each component.

    Introduction

    Multi-component heterostructure nanocomposites,which composed of two or more nanomaterials,can inherit the unique properties and overcome the limitation of single component 1-2. At the same time,the multi-component heterostructure can endow many new properties,such as magnetism,light,electricity and etc. 3-6. Photon upconversion(UC)has the ability to converting near infrared(NIR)photons into visible or ultraviolet(UV)radiation,it is a unique imaging technique that utilizes low photon energy 7-8. The UC nanomaterials are composed of matrix doped with rare earth ions used as sensitizer and activators. And modification of luminescence can be achieved by changing the type of rare earth ions. Owing to the low photon energy,high rare-earth ion solubility and good thermal stability,the rare-earth fluorides(NaREF4)are the most effective matrix. NaGdF4 is as candidate own to lower vibrational phonon energy and matching lattice with doped ions 9-10. Besides,the hexagonal phase NaGdF4 can improve the luminous efficiency of UC,and Gd3+ has a large energy level interval,it can also pass sensitization ion(Yb3+)and activation ion(Er3+,Tm3+ and Ho3+)achieves high-efficiency UC luminescence. Er3+ has fluorescence response of blue,green and red light,and the emission could be adjusted by tuning structure. Therefore,NaGdF4:Yb,Er has the advantages of low excitation energy,high luminous efficiency and good thermal stability,so it has potential application prospects in biological imaging,drug delivery,tumor treatment,display equipment,solar energy conversion,etc.11-12. However,NaGdF4:Yb,Er has a tendency to aggregate and quench,which greatly reduces its photoluminescence(PL)performance,and the oil phase system limits its application. Meanwhile,realizing the tuning of light is expected to broaden the application range of NaGdF4:Yb,Er. In order to make up for its shortcomings,many strategies had been reported,such as forming core-shell structure,tuning size or morphology and constructing the composites13-15. Among many methods,construction heterostructure by compounding with other materials can not only improve the stability and compatibility of NaGdF4:Yb,Er,but also tuning optical properties.

    Metal-organic frameworks(MOFs)are a class of carrier materials with unprecedented chemical and structural tunability. Their synthetic controllability and structural design properties make MOFs as ideal platforms for identifying design features for advanced functional materials16. Meanwhile,MOFs are considered as promising energy transmission(ET)platform to achieve collaborative molecular level functions and promote efficient energy transfer due to the highly accessible and spatially discrete linkers17. Li et al. integrated UC nanoparticles and MOF to construct a composite photocatalyst that has adjustable photocatalytic activity18. Chen et al. prepared core-shell UC nanoparticle@MOF nanoprobes for luminescent/magnetic dual-mode targeted imaging13. In our work,MIL-101/NaGdF4:Yb,Er were prepared by the two-step method,the photocatalyst displayed higher photocurrent and better degradation ability for Rhodamine B owing to synergistic effect14. Those works make full use of the adsorption and good bio-compatibility of MOFs. Zeolitic imidazolate frameworks(ZIFs)is a nitrogen-containing MOFs material obtained by compounding an imidazole or purine organic ligand with a transition metal ion. In particular,ZIF-67 is a regular dodecahedral structure material containing Co2+,it has the advantages of high stability,high porosity,and large specific surface area19. The multiple energy levels contained in Co2+ can meet the energy exchange requirements with rare earth ions20. Therefore,construction heterostructure containing ZIF-67 is an effective strategy to broaden the application prospect of NaGdF4:Yb,Er while achieving light tuning.

    Here in,we have prepared multi-component heterostructure ZIF-67/NaGdF4:Yb,Er by a stepwise synthesis method. The NaGdF4:Yb,Er nanorods were loaded on the surface of ZIF-67,which was used as a carrier. The heterostructure ZIF-67/NaGdF4:Yb,Er,which avoided agglomeration and quench of UC nanoparticles,display better stability. Meanwhile,the composites improved the compatibility of alcohol,so that it broke through the constraints of oil phase systems. ZIF-67 is also used as an ET platform to achieve UC PL tuning of NaGdF4:Yb,Er nanorods by energy transition. Compared with NaGdF4:Yb,Er nanorods under 980 nm laser excitation,the PL performance of heterostructure ZIF-67/NaGdF4:Yb,Er has converted from green light to red light that owing to the synergistic effect between individual components. The incorporation of ZIF-67 alter the PL performance of NaGdF4:Yb,Er nanorods and lead to a heterostructure with good stability,which broadens the application and promotes the progress of key technologies in the field of photon UC nanomaterials.

    1 Experiments

    1.1 Synthesis of NaGdF4:Yb,Er upconversion nanoparticles

    In a typical preparation,1.2 g NaOH was dissolved in 2 ml deionized water and ultrasonically dispersed. After the heat released,the solution was heating and stirring in a 50 ℃ water bath. Next,8 ml alcohol and 20 ml oleic acid were added to the above solution under stirring 20 min to be a transparent solution. 1 mmol of Ln(NO33·6H2O(Ln:78% Gd;20% Yb;2% Er)aqueous solution were added under vigorous stirring. Then,0.8 g PVP dissolved in 3 ml of ethanol and add to above solution. Subsequently,8 ml of NaF aqueous solution(1 mol/L)was added dropwise to the solution. Keep stirring to give it had a good dispersion to form a translucent colloidal solution. Finally,the mixed solution was transferred into reaction kettle and heated at 180 ℃ for 18 h. After reaction was completed,the system was cooled to room temperature naturally. The prepared samples were separated and washed used deionized water and ethanol by centrifugation to remove oleic acid and other remnants,and was stored in cyclohexane solvent.

    1.2 Synthesis of ZIF-67

    0.2911g of Co(NO32·6H2O and 0.3284 g of 2-methylimidazole was dissolved in 25 ml of methanol and ultrasound for 10 min,respectively. Then the dissolved 2-methylimidazole solution was added dropwise to the Co(NO32·6H2O solution,and stirred at room temperature for 3 h. Finally,the samples were separated to remove other remnants and stored in methanol.

    1.3 Synthesis of the heterostructure ZIF-67/NaGdF4:Yb,Er

    Briefly,the prepared NaGdF4:Yb,Er nanorods and ZIF-67 were mixed together. And then some PVP was added as dispersant,the mixture were stirred at 50 ℃ for 24 h. Finally,the samples were separated and washed to remove other remnants and stored in methanol.

    2 Results and discussions

    As showed in Fig. 1,firstly,the NaGdF4:Yb,Er nanorods was prepared at 180℃ and react for 18 h by hydrothermal treatment,which experience three-stage is nucleation,growth and regrowth during the reaction. And then,NaGdF4:Yb,Er nanorods were added into ZIF-67,which prepared at room temperature for 3 h. Meanwhile,some PVP was added in the mixture as dispersant to prevent NaGdF4:Yb,Er nanorods from aggregation. Finally,this mixture was string at 50℃ for 24 h to obtained heterostructure ZIF-67/NaGdF4:Yb,Er. The detailed information of experiment could be found from Supplementary material

    Illustration for the preparation of heterostructure ZIF-67/NaGdF4: Yb, Er

    Figure 1.Illustration for the preparation of heterostructure ZIF-67/NaGdF4: Yb, Er

    The morphology of samples are characterized via transmission electron microscopy(TEM). As shown in Fig. 2(a),the length of prepared NaGdF4:Yb,Er nanorods are around 50 nm. And the corresponding high-resolution transmission electron microscopy(HRTEM)image(inset of Fig. 2(a))reveals clear lattice fringes with an inter-planar spacing of 0.49 nm,which is ascribed to the(101)plane of β-NaGdF4:Yb,Er. The result was consistent with hexagonal phase(PDF:27-0699),and determined by X-ray diffraction(XRD)(Fig. 3(a)). The size of ZIF-67 was approximately 500 nm,and it exhibited a typical and regular dodecahedron(Fig. 2(b)). As shown in Fig. 2(c-d),the NaGdF4:Yb,Er nanorods are uniformly loaded on the surface of ZIF-67,and it was confirmed to be NaGdF4:Yb,Er nanorods by HRTEM(Inset of Fig. 2(d)). Furthermore,as shown in energy dispersive X-ray spectroscopy(EDS),the Co element(from ZIF-67)was mainly distributed in the inside,and the F,Gd,Yb and Er elements(from NaGdF4:Yb,Er nanorods)were homogeneously distributed throughout the heterostructure(Fig. 2(e)). And the Fourier transform infrared(FT-IR)spectra(Fig. 3(b))evidenced the formation of heterostructure in ZIF-67/NaGdF4:Yb,Er,this is consistent with the TEM and EDS results. From above analysis,the heterostructure ZIF-67/NaGdF4:Yb,Er was prepared successfully.

    The morphological characterization of heterostructure ZIF-67/NaGdF4: Yb, Er (a) TEM image of NaGdF4: Yb, Er nanorods, the inset is HRTEM image taken from (a) , (b) TEM image of ZIF-67, (c) TEM image of heterostructure ZIF-67/NaGdF4: Yb, Er, the inset is 3D model of (c) , (d) The partial enlargement of (c) , the inset is HRTEM image taken from (c) , (e) EDS elemental mapping of heterostructure ZIF-67/NaGdF4: Yb, Er.

    Figure 2.The morphological characterization of heterostructure ZIF-67/NaGdF4: Yb, Er (a) TEM image of NaGdF4: Yb, Er nanorods, the inset is HRTEM image taken from (a) , (b) TEM image of ZIF-67, (c) TEM image of heterostructure ZIF-67/NaGdF4: Yb, Er, the inset is 3D model of (c) , (d) The partial enlargement of (c) , the inset is HRTEM image taken from (c) , (e) EDS elemental mapping of heterostructure ZIF-67/NaGdF4: Yb, Er.

    The XRD and FT-IR spectra of heterostructure ZIF-67/NaGdF4: Yb, Er

    Figure 3.The XRD and FT-IR spectra of heterostructure ZIF-67/NaGdF4: Yb, Er

    The UC PL properties and conversion mechanism of heterostructure ZIF-67/NaGdF4:Yb,Er were measured. As shown in Fig. 4(a),compared with PL performance of NaGdF4:Yb,Er nanorods under 980 nm laser excitation,the green light(541 nm)of heterostructure ZIF-67/NaGdF4:Yb,Er was drastically reduced and the red light(658 nm)was enhanced largely. And compared with ZIF-67,the red light has a significant enhanced,indicates that the PL tuning was attributed to the formation of the heterostructure. The absorption of heterostructure composites were further explored via UV-vis spectroscopy(Fig. 4(b)). The heterostructure ZIF-67/NaGdF4:Yb,Er exhibited a broader absorption range and higher absorption strength compared with each component. Meanwhile,a new absorption peak appeared in the green region(510 nm-630 nm)compared with NaGdF4:Yb,Er nanorods,which was contributed by ZIF-67. As shown in Fig. 4(c),the heterostructure ZIF-67/NaGdF4:Yb,Er emitted red light(658 nm)under 541 nm laser excitation owing to the synergistic effect between ZIF-67 and NaGdF4:Yb,Er nanorods. The photon energy of 541 nm was absorbed by ZIF-67 and emitted as red light(635 nm)through energy level transition,then transited to the energy level of Er3+ through photon relaxation,finally appeared as 658 nm emission of Er3+. This mechanism will be further discussed in Fig. 6. Benefiting from the construction of heterostructure,this ZIF-67/NaGdF4:Yb,Er achieved PL tuning and improved intensity of luminescence,which broadens its scope of application.

    Characterization and comparison of fluorescence properties of heterostructure ZIF-67/NaGdF4: Yb, Er (a) UC PL spectra under 980 nm laser excitation, (b) UV-vis spectra, (c) PL emission spectra of heterostructure ZIF-67/NaGdF4: Yb, Er, the inset is PL emission spectra of NaGdF4: Yb, Er nanorods and ZIF-67, (d) UC PL spectra of heterostructure ZIF-67/NaGdF4: Yb, Er with different concentration of NaGdF4: Yb, Er nanorods, the inset is the variation of PL intensity

    Figure 4.Characterization and comparison of fluorescence properties of heterostructure ZIF-67/NaGdF4: Yb, Er (a) UC PL spectra under 980 nm laser excitation, (b) UV-vis spectra, (c) PL emission spectra of heterostructure ZIF-67/NaGdF4: Yb, Er, the inset is PL emission spectra of NaGdF4: Yb, Er nanorods and ZIF-67, (d) UC PL spectra of heterostructure ZIF-67/NaGdF4: Yb, Er with different concentration of NaGdF4: Yb, Er nanorods, the inset is the variation of PL intensity

    TEM images of heterostructure ZIF-67/NaGdF4: Yb, Er with different NaGdF4: Yb, Er nanorods concentration

    Figure 5.TEM images of heterostructure ZIF-67/NaGdF4: Yb, Er with different NaGdF4: Yb, Er nanorods concentration

    Schematic energy level diagram showing the UC process mechanism of heterostructure ZIF-67/NaGdF4: Yb, Er

    Figure 6.Schematic energy level diagram showing the UC process mechanism of heterostructure ZIF-67/NaGdF4: Yb, Er

    More interestingly,it found that the intensity of PL was related to the ratio of NaGdF4:Yb,Er and ZIF-67 as shown in Fig. 4 d. With the amount of NaGdF4:Yb,Er increased,the intensity of red light(658 nm)enhanced linearly and remains unchanged after reaching the maximum. This is due to saturation of NaGdF4:Yb,Er loading on ZIF-67,which could be further verified by TEM(Fig. 5). And the aggregated NaGdF4:Yb,Er nanorods could be found when the amount of NaGdF4:Yb,Er was increased after saturation(30%). Therefore,the heterostructure ZIF-67/NaGdF4:Yb,Er not only tune PL emission,but also improved stability.

    As can be seen from Fig. 4,the emission peak of the heterostructure ZIF-67/NaGdF4:Yb,Er appeared at 658 nm is corresponding to the energy level transition of Er3+. Without ZIF-67,the energy transfer process of NaGdF4:Yb,Er is as follows15:the electrons in the 2F7/2 ground state of Yb3+ are excited to the 2F5/2 excited states after absorbing the 980 nm excitation. And then the energy is transferred to 2I11/24F9/2,and 4F7/2 level of Er3+ by radiation 21. Subsequently,the energy transferred to the 4I11/2 level of Er3+ causes the electrons in this level jumped to the 4F7/2 state. And then the electrons relax rapidly to the 2H11/2 and the 4S3/2 states through multiphonon relaxation steps,leading to the green emission bands. The electrons in the 4F9/2 level of Er3+ was following nonradiative transition process to the ground state 4I15/2 of Er3+ by absorbing the additional excitation energy migrated from Yb3+ and producing the red emission 22-23. The green light emitted at 524 nm and 541 nm,which were mainly derived from 2H11/2 to 4I15/24S3/2 to 4I15/2 energy transfer,respectively 24. And the red light emitted at 658 nm is mainly derived from 4F9/2 to 4I15/2 energy transfer. For heterostructure ZIF-67/NaGdF4:Yb,Er,the new energy level is introduced from ZIF-6720. Just as the result revealed in Fig. 3(b)and 3(c),the energy at the 2H11/2 and 4S3/2 of Er3+ is transferred to S1 of Co2+(form ZIF-67). And then energy at S1 of Co2+ transferred to 4F9/2 of Er3+,so that the PL intensity enhanced linearly. New energy transfer takes place in the heterostructure ZIF-67/NaGdF4:Yb,Er,which is the key to the PL tuning and enhancement.

    3 Conclusions

    In summary,the heterostructure ZIF-67/NaGdF4:Yb,Er was prepared by a facile stepwise synthesis method,the NaGdF4:Yb,Er nanorods are uniformly loaded on the surface of ZIF-67. And the heterostructure overcame the shortcomings of NaGdF4:Yb,Er nanorods in agglomeration and quench. Under the 980 nm laser excitation,the energy transfer takes place in the heterostructure ZIF-67/NaGdF4:Yb,Er. And controllable PL tuning was realized by construction heterostructure the enhanced emission was converted from green light to red light. This strategy greatly enhances the applicability of heterostructure ZIF-67/NaGdF4:Yb,Er,break through the limitation of oil phase system of NaGdF4:Yb,Er nanorods,making it promising for biological imaging,bio-molecular detection and bio-sensor.

    References

    [1] M S Gudiksen, L J Lauhon, J F Wang et al. Growth of nanowire superlattice structures for nanoscale photonics and electronics. Nature, 415, 617-620(2002).

    [2] T Mokari, C G Sztrum, A Salant et al. Formation of asymmetric one-sided metal-tipped semiconductor nanocrystal dots and rods. Nat. Mater, 4, 855-863(2005).

    [3] X T Wang, T Ouyang, L Wang et al. Redox‐Inert Fe3+ Ions in Octahedral Sites of Co‐Fe Spinel Oxides with Enhanced Oxygen Catalytic Activity for Rechargeable Zinc–Air Batteries. Angew. Chem. Int Edit, 131, 13425-13430(2019).

    [4] Z LI, C. WANG, X Z CHEN et al. MoOx nanoparticles anchored on N-doped porous carbon as Li-ion battery electrode. Chem. Eng. J., 381(2020).

    [5] S T FAN, J ZHANG, X L TENG et al. Self-Supported Amorphous SnO2/TiO2 Nanocomposite Films with Improved Electrochemical Performance for Lithium-Ion Batteries. J. Electrochem. Soc., 166, A3072-A3078(2019).

    [6] F ZHENG, S J SUN, Y Q FENG et al. Yb:Ca9Gd(VO4)7, a potential ultrafast pulse laser crystal with promising spectral properties. J. Lumin, 221, 117085(2020).

    [7] J Q JIAO, L. A BELFIORE, W F. SHEN et al. Fabrication and luminescence of KGdF4:Yb3+/Er3+ nanoplates and their improving performance for polymer solar cells. Sci. Bull, 063, 216-218(2019).

    [8] J Q JIAO, S S. GAI, W F SHEN et al. NaYbF4:Tb/Eu modified with organic antenna for improving performance of polymer solar cells. Electrochim. Acta, 260, 959-964(2018).

    [9] Y LI, J Q JIAO, P L YAN et al. Synthesis and tunable photoresponse for core-shell structured NaGdF4:Yb,Er@SiO2@Eu(TTA)3Phen nanocomplexes. Scripta Mater, 152, 1-5(2018).

    [10] Y Q ZHANG, S XU, X P LI et al. Improved LRET-based detection characters of Cu2+ using sandwich structured NaYF4@ NaYF4:Er3+/Yb3+@NaYF4 nanoparticles as energy donor. Sensors Actuators B: Chemical, 257, 829-838(2018).

    [11] F Y LIU, X X HE, L LIU et al. Conjugation of NaGdF4 upconverting nanoparticles on silica nanospheres as contrast agents for multi-modality imaging. Biomaterials, 34, 5218-5225(2013).

    [12] Z H XU, C X Li, P P YANG et al. Rare Earth Fluorides Nanowires/Nanorods Derived from Hydroxides: Hydrothermal Synthesis and Luminescence Properties. Cryst. Growth Des, 9, 4752-4758(2009).

    [13] Y T LI, J L TANG, L C HE et al. Core-Shell Upconversion Nanoparticle@Metal-Organic Framework Nanoprobes for Luminescent/Magnetic Dual-Mode Targeted. Adv. Mater, 27, 4075-4080(2015).

    [14] B Z Lv, J Q JIAO, Y LIU et al. Heterostructure NaGdF4:Yb,Er anchored on MIL-101 for promoting photoelectronic response and photocatalytic activity. Nanoscale, 11, 22730-22733(2019).

    [15] C L YAN, A. DADVAND, F. ROSEI et al. Near-IR photoresponse in new up-converting CdSe/NaYF4:Yb,Er nanoheterostructures. J. Am. Chem. Soci, 132, 8868-8869(2010).

    [16] A. E. Baumann, D. A. Burns, B Q LIU et al. Metal-organic framework functionalization and design strategies for advanced electrochemical energy storage devices. Commun. Chem, 2, 86(2019).

    [17] M. HOSOYAMADA, A N. YAN, K. Okumura et al. Translating MOF chemistry into supramolecular chemistry: soluble coordination nanofibers showing efficient photon upconversion. Chem. Commun, 54, 6828-6831(2018).

    [18] M H LI, Z J ZHENG, Y Q ZHENG et al. Controlled Growth of Metal-Organic Framework on Upconversion Nanocrystals for NIR-Enhanced Photocatalysis. ACS Appl. Mater. Inter, 9, 2899-2905(2017).

    [19] W Y LI, F YANG, X J Fang et al. Systematic post-synthetic modification of metal-organic framework (ZIF-67) with superior cyclability for lithium-ion batteries. Electrochim. Acta, 282, 276-285(2018).

    [20] J. ERGUSON, D. L. WOOD, L UITERT. G. V. Crystal-field spectra of d3,7 ions. V. Tetrahedral CO2+ in ZnAl2O4 Spinel. J. Chem. Phys, 51, 2904-2910(1969).

    [21] P DU, L H LUO, J S YU. Controlled synthesis and upconversion luminescence of Tm3+-doped NaYbF4 nanoparticles for non-invasion optical thermometry. J. Alloy. Compd, 739, 926-933(2018).

    [22] J TANG, C LI, J LI et al. Selectively enhanced red upconversion luminescence and phase/size manipulation via Fe3+ doping in NaYF4:Yb,Er nanocrystals. Nanoscale, 7, 14752-14759(2015).

    [23] Q ZHU, C Y SONG, X D LI et al. Up-conversion monodispersed spheres of NaYF4:Yb3+/Er3+: green and red emission tailoring mediated by heating temperature, and greatly enhanced luminescence by Mn2+ doping. J. Chem. Soc. Dalton, 47, 8646-8655(2018).

    [24] Y Y TIAN, Y TIAN, P HUANG et al. Effect of Yb3+ concentration on upconversion luminescence and temperature sensing behavior in Yb3+/Er3+ co-doped YNbO4 nanoparticles prepared via molten salt route. Chem. Eng. J., 297, 26-34(2016).

    Yi LIU, Ji-Qing JIAO, Bai-Ze LYU, Jiu-Xing WANG. The heterostructure NaGdF4:Yb,Er nanorods loaded on metal-organic frameworks for tuning upconversion photoluminescence[J]. Journal of Infrared and Millimeter Waves, 2021, 40(2): 166
    Download Citation