1. Microstructures of 2D SiC/SiC composites specimen
2. SEM image (a) and EDS analysis (b) of the 2D SiC/SiC composites with surface scans of C (c), O (d) and Si (e)
3. Diagram of the high-temperature system under inert gas environment
4. Equipment of uniaxial tensile experiment of 2D SiC/SiC composites specimen
5. 2D SiC/SiC composites specimen
6. Resistivity-temperature response of the 2D SiC/SiC composites
7. Microstructures of the 2D SiC/SiC composites specimen after oxidation
8. SEM image and EDS analysis of the cross-section of the 2D SiC/SiC composites specimen after oxidation
9. Relationship between resistivity and SiO2 content of the 2D SiC/SiC composites
10. Response of resistivity and stress to strain of the 2D SiC/SiC composites
11. Response of resistivity-rate and stiffness to strain of the 2D SiC/SiC composites
12. Fracture micromorphologies of the 2D SiC/SiC composites specimen
Number | Temperature/℃ | Holding time/h | Dimension/mm |
---|
T1 | 1300 | - | 120×8 | T2 | 1300 | 20 | 60×8 | T3 | 1300 | 60 | 60×8 | T4 | - | - | 120×12 |
|
Table 1. Details of the 2D SiC/SiC composites specimens