• Bulletin of the Chinese Ceramic Society
  • Vol. 41, Issue 8, 2644 (2022)
GAO Qiang1, MEI Kaiyuan1、2, WANG Dekun3, ZHANG Liwei2, ZHANG Chunmei1, and CHENG Xiaowei1
Author Affiliations
  • 1[in Chinese]
  • 2[in Chinese]
  • 3[in Chinese]
  • show less
    DOI: Cite this Article
    GAO Qiang, MEI Kaiyuan, WANG Dekun, ZHANG Liwei, ZHANG Chunmei, CHENG Xiaowei. CO2 Corrosion Kinetics of C3S in Cement Single Ore under CCUS Environment[J]. Bulletin of the Chinese Ceramic Society, 2022, 41(8): 2644 Copy Citation Text show less
    References

    [1] CHANG Y S, LEE J, YOON H. Alternative projection of the world energy consumption-in comparison with the 2010 international energy outlook[J]. Energy Policy, 2012, 50: 154-160.

    [3] GLEICK P H. Erratum: climate change and the integrity of science (science (689)) (erratum)[J]. Science, 2010(5980): 826.

    [4] BACHU S. CO2 storage in geological media: role, means, status and barriers to deployment[J]. Progress in Energy and Combustion Science, 2008, 34(2): 254-273.

    [5] BRANDO N B, ROEHL D, DE ANDRADE S F, et al. The impact of cement slurry aging creep on the construction process of oil wells[J]. Journal of Petroleum Science and Engineering, 2017, 157: 422-429.

    [8] OMOSEBI O, MAHESHWARI H, AHMED R, et al. Degradation of well cement in HPHT acidic environment: effects of CO2 concentration and pressure[J]. Cement and Concrete Composites, 2016, 74: 54-70.

    [9] OMOSEBI O, MAHESHWARI H, AHMED R, et al. Investigating temperature effect on degradation of well cement in HPHT carbonic acid environment[J]. Journal of Natural Gas Science and Engineering, 2015, 26: 1344-1362.

    [10] DONG S J, BERELSON W M, ROLLINS N E, et al. Aragonite dissolution kinetics and calcite/aragonite ratios in sinking and suspended particles in the North Pacific[J]. Earth and Planetary Science Letters, 2019, 515: 1-12.

    [11] SNCHEZ-HERRERO M J, FERNNDEZ-JIMNEZ A, PALOMO . Alkaline hydration of C2S and C3S[J]. Journal of the American Ceramic Society, 2016, 99(2): 604-611.

    [12] CUESTA A, ZEA-GARCIA J D, LONDONO-ZULUAGA D, et al. Multiscale understanding of tricalcium silicate hydration reactions[J]. Scientific Reports, 2018, 8: 8544.

    [13] MEI K Y, CHENG X W, ZHANG H, et al. The coupled reaction and crystal growth mechanism of tricalcium silicate (C3S): an experimental study for carbon dioxide geo-sequestration wells[J]. Construction and Building Materials, 2018, 187: 1286-1294.

    [14] GU T, GUO X Y, LI Z Y, et al. Coupled effect of CO2 attack and tensile stress on well cement under CO2 storage conditions[J]. Construction and Building Materials, 2017, 130: 92-102.

    [15] BAI M X, SUN J P, SONG K P, et al. Well completion and integrity evaluation for CO2 injection wells[J]. Renewable and Sustainable Energy Reviews, 2015, 45: 556-564.

    [16] WEICHMANN M J, REINICKE K M. Risk assessment of abandoned wells affected by CO2[J]. Erdol Erdgas Kohle, 2016(9): A125-A129.

    [17] BAI M X, ZHANG Z C, FU X F. A review on well integrity issues for CO2 geological storage and enhanced gas recovery[J]. Renewable and Sustainable Energy Reviews, 2016, 59: 920-926.

    [18] KLIMAVICIUS V, HILBIG H, GUTMANN T, et al. Direct observation of carbonate formation in partly hydrated tricalcium silicate by dynamic nuclear polarization enhanced NMR spectroscopy[J]. The Journal of Physical Chemistry C, 2021, 125(13): 7321-7328.

    [19] WANG D, XIONG C, LI W Z, et al. Growth of calcium carbonate induced by accelerated carbonation of tricalcium silicate[J]. ACS Sustainable Chemistry & Engineering, 2020, 8(39): 14718-14731.

    [20] MEI K Y, CHENG X W, GU T, et al. Effects of Fe and Al ions during hydrogen sulphide (H2S)-induced corrosion of tetracalcium aluminoferrite (C4AF) and tricalcium aluminate (C3A)[J]. Journal of Hazardous Materials, 2021, 403: 123928.

    [21] GOMEZ-VILLALBA L S, LPEZ-ARCE P, DE BUERGO M A, et al. Atomic defects and their relationship to aragonite-calcite transformation in portlandite nanocrystal carbonation[J]. Crystal Growth & Design, 2012, 12(10): 4844-4852.

    [25] GROVES G W, BROUGH A, RICHARDSON I G, et al. Progressive changes in the structure of hardened C3S cement pastes due to carbonation[J]. Journal of the American Ceramic Society, 1991, 74(11): 2891-2896.

    [26] DOLADO J S, ZHU W, HERNNDEZ M S, et al. Textural and mechanical characterization of C-S-H gels from hydration of synthetic T1-C3S, β-C2S and their blends[J]. Materiales de Construccion, 2011: 169-183.

    [29] KNOPF F C, ROY A, SAMROW H A, et al. High-pressure molding and carbonation of cementitious materials[J]. Industrial & Engineering Chemistry Research, 1999, 38(7): 2641-2649.

    [30] REARDON E J, JAMES B R, ABOUCHAR J. High pressure carbonation of cementitious grout[J]. Cement and Concrete Research, 1989, 19(3): 385-399.

    [31] SHAH V, SCRIVENER K, BHATTACHARJEE B, et al. Changes in microstructure characteristics of cement paste on carbonation[J]. Cement and Concrete Research, 2018, 109: 184-197.

    [32] JIMOH O A, ARIFFIN K S, HUSSIN H B, et al. Synthesis of precipitated calcium carbonate: a review[J]. Carbonates and Evaporites, 2018, 33(2): 331-346.

    [33] CHESHIRE M C, STACK A G, CAREY J W, et al. Wellbore cement porosity evolution in response to mineral alteration during CO2 flooding[J]. Environmental Science & Technology, 2017, 51(1): 692-698.

    [35] AUROY M, POYET S, LE BESCOP P, et al. Impact of carbonation on unsaturated water transport properties of cement-based materials[J]. Cement and Concrete Research, 2015, 74: 44-58.

    GAO Qiang, MEI Kaiyuan, WANG Dekun, ZHANG Liwei, ZHANG Chunmei, CHENG Xiaowei. CO2 Corrosion Kinetics of C3S in Cement Single Ore under CCUS Environment[J]. Bulletin of the Chinese Ceramic Society, 2022, 41(8): 2644
    Download Citation