    Guo Qingfeng, Zhang Zheng, Huang Lijie, Lin Wenxiong. Effects of Pulsed Laser on Surface Quality and Deformation of Selective Laser Melted Ti6Al4V Titanium Alloy[J]. Laser & Optoelectronics Progress, 2020, 57(21): 211404 Copy Citation Text show less
    SEM image of TC4 titanium alloy powder
    Fig. 1. SEM image of TC4 titanium alloy powder
    Relative density of TC4 titanium samples under different laser parameters
    Fig. 2. Relative density of TC4 titanium samples under different laser parameters
    SEM images of TC4 titanium samples under different pulse duty cycles. (a)--(d) Pulse duty cycle is 30%, 50%, 60%, 100%, when the laser power is 110 W; (e)--(f) pulse duty cycle is 30%, 80 %, when the laser power is 190 W
    Fig. 3. SEM images of TC4 titanium samples under different pulse duty cycles. (a)--(d) Pulse duty cycle is 30%, 50%, 60%, 100%, when the laser power is 110 W; (e)--(f) pulse duty cycle is 30%, 80 %, when the laser power is 190 W
    Surface roughness of TC4 titanium samples under different parameters
    Fig. 4. Surface roughness of TC4 titanium samples under different parameters
    SEM images of TC4 titanium sample surface under different pulse duty cycles (laser power is 110 W).(a) 30%; (b) 50%; (c) 60%; (d) 70%; (e) 80%; (f) 100%
    Fig. 5. SEM images of TC4 titanium sample surface under different pulse duty cycles (laser power is 110 W).(a) 30%; (b) 50%; (c) 60%; (d) 70%; (e) 80%; (f) 100%
    SEM images of TC4 titanium sample surface under different pulse duty cycles (laser power is 190 W).(a) 30%; (b) 50%; (c) 60%; (d) 70%; (e) 80%; (f) 100%
    Fig. 6. SEM images of TC4 titanium sample surface under different pulse duty cycles (laser power is 190 W).(a) 30%; (b) 50%; (c) 60%; (d) 70%; (e) 80%; (f) 100%
    SEM images of TC4 titanium samples under different pulse duty cycles. (a) 30%; (b) 50%; (c) 70%; (d) 100%
    Fig. 7. SEM images of TC4 titanium samples under different pulse duty cycles. (a) 30%; (b) 50%; (c) 70%; (d) 100%
    Deformation of the printed part when the laser power is 190 W. (a) Laser with pulse duty cycle is 70%;(b) continuous laser
    Fig. 8. Deformation of the printed part when the laser power is 190 W. (a) Laser with pulse duty cycle is 70%;(b) continuous laser
    ElementTiAlVFeCHON
    Mass fraction /%Bal.6.424.000.210.00760.00160.120.004
    Table 1. Composition of TC4 titanium alloy powder