    Structural diagram of laser cleaning equipment
    Fig. 1. Structural diagram of laser cleaning equipment
    Morphology and composition analysis of rusting layer. (a) Macro morphology; (b) SEM image; (c) X-ray diffraction peak
    Fig. 2. Morphology and composition analysis of rusting layer. (a) Macro morphology; (b) SEM image; (c) X-ray diffraction peak
    Diagram of light spot lapping
    Fig. 3. Diagram of light spot lapping
    High-speed photography photos at different time under both of two laser cleaning methods. (a)-(c) Dry laser cleaning; (d)-(f) liquid film-assisted laser cleaning
    Fig. 4. High-speed photography photos at different time under both of two laser cleaning methods. (a)-(c) Dry laser cleaning; (d)-(f) liquid film-assisted laser cleaning
    Surface morphologies of laser derusting samples at different process parameters. (a)(d) 100 W; (b)(e) 300 W; (c)(f) 400 W
    Fig. 5. Surface morphologies of laser derusting samples at different process parameters. (a)(d) 100 W; (b)(e) 300 W; (c)(f) 400 W
    Surface SEM morphologies of dry laser cleaning samples under different powers. (a) 100 W; (b) 300 W; (c) 400 W
    Fig. 6. Surface SEM morphologies of dry laser cleaning samples under different powers. (a) 100 W; (b) 300 W; (c) 400 W
    Surface SEM morphologies of liquid film-assisted laser cleaning samples under different powers. (a) 100 W; (b) 300 W; (c) 400 W
    Fig. 7. Surface SEM morphologies of liquid film-assisted laser cleaning samples under different powers. (a) 100 W; (b) 300 W; (c) 400 W
    Surface roughness of sample before and after different laser cleaning methods
    Fig. 8. Surface roughness of sample before and after different laser cleaning methods
    Oxygen content of sample surface after laser cleaning
    Fig. 9. Oxygen content of sample surface after laser cleaning
    X-ray diffraction peak contrast of rusting layer and laser derusting sample
    Fig. 10. X-ray diffraction peak contrast of rusting layer and laser derusting sample