• Chinese Journal of Lasers
  • Vol. 43, Issue 4, 403001 (2016)
Wang Zhihui1、2、3、4、*, Wang Huaming1、2、3、4, and Liu Dong1、2、3、4
Author Affiliations
  • 1[in Chinese]
  • 2100191
  • 3[in Chinese]
  • 4[in Chinese]
  • show less
    DOI: 10.3788/cjl201643.0403001 Cite this Article Set citation alerts
    Wang Zhihui, Wang Huaming, Liu Dong. Microstructure and Mechanical Properties of AF1410 Ultra-High Strength Steel Using Laser Additive Manufacture Technique[J]. Chinese Journal of Lasers, 2016, 43(4): 403001 Copy Citation Text show less
    References

    [1] Xu Changgan, Zhang Shaorui. Ultra-high strength steel AF1410 with high toughness[J]. Special Steel, 1993, 14(6): 11-14.

    [2] Grujicic M. Coherent precipitation of M2C carbides in AF1410 steel[J]. Materials Science & Engineering A, 1989, 117(5): 215-220.

    [3] Yu Wei, Han Peng, Wu Bing. Influence of pre-corrosion on fatigue property of AF1410 EBW joint[J]. Aeronautical Manufacturing Technology, 2010, (20): 86-88.

    [4] Lu Bingheng, Li Dichen. Development of the additive manufacturing (3D printing) technology[J]. Machine Building & Automation, 2013, 42(4): 1-4.

    [5] Shi Yusheng, Li Ruidi, Zhang Wenxian, et al.. Study on rapid prototyping process of stainless steel powder by selective laser melting[J]. Rapid Pprototyping and Rapid Manufacturing Technology, 2010, B04(1): 67-72.

    [6] Zhao Jianfeng, Ma Zhiyong, Xie Deqiao, et al.. Metal additive manufacturing technique[J]. Journal of Nanjing University of Aeronautics & Astronautics, 2014, 46(5): 675-683.

    [7] Wang Huaming, Zhang Shuquan, Wang Xiangming. Progress and challenges of laser direct manufacturing of large titanium structural components (invited paper)[J]. Chinese J Lasers, 2009, 36(12): 3204-3209.

    [8] Chen Yongcheng, Zhang Shuquan, Tian Xiangjun, et al.. Microstructure and micro-hardness of 4045 Aluminum alloy fabricated by laser melting deposition[J]. Chinese J Lasers, 2015, 42(3): 0303008.

    [9] Jiang Hua, Tang Haibo, Fang Yanli, et al.. Microstructure and mechanical properties of rapid solidified ultra-fine columnar grain Nibase superalloy DZ408 by laser melting deposition manufacturing[J]. Chinese J Lasers, 2012, 39(2): 0203004.

    [10] Feng Shurong, Zhang Shuquan, Wang Huaming. Wear resistance of laser clad hard particles reinforced intermetallic composite coating on TA15 Alloy[J]. Chinese J Lasers, 2012, 39(2): 0203002.

    [11] Handerhan K J, Garrison W M, Moody N R. A comparison of the fracture behavior of two heats of the secondary hardening steel AF1410 [J]. Metallurgical & Materials Transactions A, 1989, 20(1): 105-123.

    [12] Garrison W M, Moody N R. Influence of inclusion spacing and microstructure on the fracture toughness of the secondary hardening steel AF1410[J]. Metallurgical & Materials Transactions A, 1987, 18(7): 1257-1263.

    [13] Lee K B, Kwon H, Kwon H, et al.. Effects of alloying additions and austenitizing treatments on secondary hardening and fracture behavior for martensitic steels containing both Mo and W[J]. Metallurgical & Materials Transactions A, 2001, 32(7): 1659-1670.

    [14] Li Ani, Li Yong, Wang Chunxu, et al.. Influence of Mo on secondary hardening behavior of ultra-high strength AF1410 steel[J]. Iron and Steel, 2007, 42(9): 60-62.

    [15] Davis J R. ASM handbook[M]. Allama Iqbal Town: ASM International, 2003: 733-735.

    [16] Sun Xiaomin, Liu Dong, Tang Haibo, et al.. Solid-state phase transformation and microstructure of laser direct manufactured TC17 titanium alloy components[J]. Rare Metal Materials and Engineering, 2013, 42(4): 724-729.

    [17] Han Shun, Li Yong, Wang Chunxu, et al.. Behavior of rotating-bending fatigue failure of AF1410 steel[J]. Iron and Steel, 2013, 48(3): 82-85.

    [18] Zhong Qunpeng, Zhao Zihua. Fractography[M]. Beijing: High Education Press, 2006.

    [19] Gan Yong, Tian Zhiling, Dong Han, et al.. Chinese Materials Engineering Canon[M]. Beijing: Chemical Industry Press, 2005.

    [20] Cui Zhongqi, Tan Yaochun. Metallurgy and heat treatment[M]. Beijing: China Machine Press, 2010.

    CLP Journals

    [1] Ren Chao, Li Zhuguo, Shu Da, Zhao Wenyu, Yang Renjie, Wang Peng, Ye Jianshui. Microstructure and Water Erosion Resistance Property of Stellite6 Coating by Laser Cladding on 17-4PH Stainless Steel Surface[J]. Chinese Journal of Lasers, 2017, 44(4): 402010

    [2] Jiao Shikun, Liu Shaoyin, Liu Dong, Cheng Xu. Heat Treatment Microstructures and TB Phase Precipitation of Laser Additive Manufactured Al-Li Alloys[J]. Chinese Journal of Lasers, 2018, 45(5): 502001

    [3] Liu Jiahe, Zhu Haihong, Hu Zhiheng, Ke Linda, Zeng Xiaoyan. Control of Elevated Edge in Selective Laser Melt Molding[J]. Chinese Journal of Lasers, 2017, 44(12): 1202007

    [4] Liu Xiaoxin, Cheng Xu, Wang Huaming, Li Jia. Influence of Processing Conditions on Formation of Stray Grains in DD5 Single-Crystal Superalloys by Laser Melting Multi-Traced Deposition[J]. Chinese Journal of Lasers, 2017, 44(6): 602009

    [5] Liu Zhengwu, Cheng Xu, Li Jia, Wang Huaming. Heat-Processing Technology for Laser Additive Manufacturing of 05Cr15Ni5Cu4Nb Precipitation-Hardening Stainless Steels[J]. Chinese Journal of Lasers, 2017, 44(6): 602010

    Wang Zhihui, Wang Huaming, Liu Dong. Microstructure and Mechanical Properties of AF1410 Ultra-High Strength Steel Using Laser Additive Manufacture Technique[J]. Chinese Journal of Lasers, 2016, 43(4): 403001
    Download Citation