[1] X. Tong, H. Zhou, W. Jiang et al.. Study on preheating and annealing treatments to biomimetic non-smooth cast iron sample with high thermal fatigue resistance[J]. Materials Science and Engineering A, 2009, 513-514(0): 294~301
[2] A. Liu, B. Previtali. Laser surface treatment of grey cast iron by high power diode laser[J]. Physics Procedia, 2010, 5: 439~448
[3] Wang Hongying, Yao Yuan, Hu Jiandong. Parameter optimizing and microstructure analysis of laser treated gray cast iron for ca141 engine body[J]. Hot Working Process, 2004, 33(5): 339~343
[4] Ju Yi, Guo Shaoyi, Li Zhongquan. Status and development of laser surface alloying and laser cladding in China[J]. Materials Science & Engineering, 2002, 20(1): 143~145
[5] Zhou Zhenfeng. Welding Metallurgy and Technology of Cast Irons[M]. Beijing: China Machine Press, 2001. 163~205
[6] Xu Binshi. Theory and Technology of Remanufactured Equipments Engineering[M]. Beijing: National Defense Industry Press, 2007. 292~301
[7] Gu Shengting, Chai Guozhong, Yao Jianhua et al.. Laser caldding of elasto plastical properties of particle reinforced H13-TiC composite coatings[J]. Chinese J. Lasers, 2011, 38(6): 0603019
[8] Wang Yanfang, Li Li, Lu Qinglong et al.. Laser cladding Fe based amorphous coatings on stainless substrate[J]. Chinese J. Lasers, 2011, 38(6): 0603017
[9] Zhou Zhenfeng. Welding Metallurgy[M]. Beijing: China Machine Press, 1993. 105~106
[10] Pierce Villars, Alan Prinee, Hiroaki Okamoto. Handbook of Ternary Alloy Phase Diagram[M]. Materials Park OH: ASM International, 1995. 648
[11] Wen Peng, Shinozaki Kenji, Yamamoto Motomich. Evaluation of solidification cracking susceptibility during laser welding byin-situobservation method[J]. Chinese J. Lasers, 2011, 38(6): 0603005