  • Vol. 48, Issue 18, 1802004 (2021)
Wei Wang1, Jie Shen1, Weijun Liu1、*, Hongyou Bian1, Qiang Li1, and Yu Zhou2
Author Affiliations
  • 1School of Mechanical Engineering, Shenyang University of Technology, Shenyang, Liaoning 110870, China
  • 2Shenyang Pakalaijing Co., Ltd., Shenyang, Liaoning 110042, China
  • show less
    DOI: 10.3788/CJL202148.1802004 Cite this Article Set citation alerts
    Wei Wang, Jie Shen, Weijun Liu, Hongyou Bian, Qiang Li, Yu Zhou. Effect of Scanning Speed of Galvanometer on Surface Oxide Layer of TA15 Titanium Alloy in Pulsed Laser Cleaning[J]. Chinese Journal of Lasers, 2021, 48(18): 1802004 Copy Citation Text show less
    Surface morphologies of TA15 titanium alloy before and after laser cleaning. (a) Cleaned surface morphology and original surface morphology; (b) SEM image of original surface
    Fig. 1. Surface morphologies of TA15 titanium alloy before and after laser cleaning. (a) Cleaned surface morphology and original surface morphology; (b) SEM image of original surface
    Laser cleaning schematic
    Fig. 2. Laser cleaning schematic
    Scanning path of laser spot
    Fig. 3. Scanning path of laser spot
    Surface morphologies of TA15 after laser cleaning. (a) V=7000 mm·s-1; (b) V=8000 mm·s-1; (c) V=9000 mm·s-1; (d) V=10000 mm·s-1
    Fig. 4. Surface morphologies of TA15 after laser cleaning. (a) V=7000 mm·s-1; (b) V=8000 mm·s-1; (c) V=9000 mm·s-1; (d) V=10000 mm·s-1
    SEM morphologies of TA15 surface after laser cleaning. (a) V=7000 mm·s-1; (b) V=8000 mm·s-1; (c) V=9000 mm·s-1; (d) V=10000 mm·s-1
    Fig. 5. SEM morphologies of TA15 surface after laser cleaning. (a) V=7000 mm·s-1; (b) V=8000 mm·s-1; (c) V=9000 mm·s-1; (d) V=10000 mm·s-1
    Schematic of laser removal of oxide layer and oil pollution on TA15 surface
    Fig. 6. Schematic of laser removal of oxide layer and oil pollution on TA15 surface
    EDS patterns and EDS analysis of TA15 surface after laser cleaning. (a) V=7000 mm·s-1; (b) V=8000 mm·s-1; (c) V=9000 mm·s-1; (d) V=10000 mm·s-1
    Fig. 7. EDS patterns and EDS analysis of TA15 surface after laser cleaning. (a) V=7000 mm·s-1; (b) V=8000 mm·s-1; (c) V=9000 mm·s-1; (d) V=10000 mm·s-1
    XRD spectra of TA15 surface after laser cleaning
    Fig. 8. XRD spectra of TA15 surface after laser cleaning
    Hardness chart of TA15 surface after laser cleaning
    Fig. 9. Hardness chart of TA15 surface after laser cleaning
    NumberLaser powerP /WScanning speedV /(mm·s-1)Spot diameterD /mmOverlap ratio λ /%
    120070001.270.8
    220080001.266.7
    320090001.262.5
    4200100001.258.3
    Table 1. Laser cleaning process parameters
    Wei Wang, Jie Shen, Weijun Liu, Hongyou Bian, Qiang Li, Yu Zhou. Effect of Scanning Speed of Galvanometer on Surface Oxide Layer of TA15 Titanium Alloy in Pulsed Laser Cleaning[J]. Chinese Journal of Lasers, 2021, 48(18): 1802004