• Journal of Inorganic Materials
  • Vol. 36, Issue 10, 1097 (2021)
Yiming LEI1、2, Jie ZHANG1、*, Guanghai BAI3, Yanwei ZHANG3, Xiaohui WANG1, and Jingyang WANG1
Author Affiliations
  • 11. Shenyang National Laboratory for Materials Science, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, China
  • 22. School of Materials Science and Engineering, University of Science and Technology of China, Shenyang 110016, China
  • 33. Life Management Technology Center, Suzhou Nuclear Power Research Institute, China Nuclear Power Technology Research Institute, Suzhou 215004, China
  • show less
    DOI: 10.15541/jim20210029 Cite this Article
    Yiming LEI, Jie ZHANG, Guanghai BAI, Yanwei ZHANG, Xiaohui WANG, Jingyang WANG. Influence of Al Content on Oxidation Resistance of Phase-pure Ti2AlC under Simulated Loss-of-coolant Accident Conditions [J]. Journal of Inorganic Materials, 2021, 36(10): 1097 Copy Citation Text show less
    References

    [1] A TERRANI K. Accident tolerant fuel cladding development: promise, status, and challenges. Journal of Nuclear Materials, 501, 13-30(2018).

    [2] J ZINKLE S, A TERRANI K, C GEHIN J et al. Accident tolerant fuels for LWRs: a perspective. Journal of Nuclear Materials, 448, 374-379(2014).

    [3] B REBAK R. Accident Tolerant Materials for Light Water Reactor Fuels, 1st edition. Netherlands: Elsevier, 63-81(2020).

    [4] Z DUAN, H YANG, Y SATOH et al. Current status of materials development of nuclear fuel cladding tubes for light water reactors. Nuclear Engineering and Design, 316, 131-150(2017).

    [5] G KIM H, H KIM I, I JUNG Y et al. Out-of-pile performance of surface-modified Zr cladding for accident tolerant fuel in LWRs. Journal of Nuclear Materials, 510, 93-99(2018).

    [6] G KIM H, H KIM I, I JUNG Y et al. Adhesion property and high-temperature oxidation behavior of Cr-coated Zircaloy-4 cladding tube prepared by 3D laser coating. Journal of Nuclear Materials, 465, 531-539(2015).

    [7] C BRACHET J, I IDARRAGA T, L FLEM M et al. Early studies on Cr-Coated Zircaloy-4 as enhanced accident tolerant nuclear fuel claddings for light water reactors. Journal of Nuclear Materials, 517, 268-285(2019).

    [8] J TALLMAN D, B ANASORI, W BARSOUM M. A critical review of the oxidation of Ti2AlC, Ti3AlC2 and Cr2AlC in air. Materials Research Letters, 1, 115-125(2013).

    [9] H WANG X, C ZHOU Y. Layered machinable and electrically conductive Ti2AlC and Ti3AlC2 ceramics: a review. Journal of Materials Science & Technology, 26, 385-416(2010).

    [10] Y NIU, S FU, K ZHANG et al. Synthesis, microstructure, and properties of high purity Mo2TiAlC2 ceramics fabricated by spark plasma sintering. Journal of Advanced Ceramics, 9, 759-768(2020).

    [11] E OPILA, N JACOBSON, D MYERS et al. Predicting oxide stability in high-temperature water vapor. The Journal of The Minerals,Metals & Materials Society, 58, 22-28(2006).

    [12] E OPILA, D MYERS. Alumina volatility in water vapor at elevated temperatures. Journal of the American Ceramic Society, 87, 1701-1705(2003).

    [13] C TANG, M STEINBRUECK, M STUEBER et al. Deposition, characterization and high-temperature steam oxidation behavior of single-phase Ti2AlC-coated Zircaloy-4. Corrosion Science, 135, 87-98(2018).

    [14] W LI, Z WANG, J SHUAI et al. A high oxidation resistance Ti2AlC coating on Zirlo substrates for loss-of-coolant accident conditions. Ceramics International, 45, 139-139(2019).

    [15] X LI, Y QIAN, L ZHENG et al. Determination of the critical content of Al for selective oxidation of Ti3AlC2 at 1100℃. Journal of the European Ceramic Society, 36, 3311-3318(2016).

    [16] J WANG, Y ZHOU, T LIAO et al. A first-principles investigation of the phase stability of Ti2AlC with Al vacancies. Scripta Materialia, 58, 227-230(2008).

    [17] J FRODELIUS, P EKLUND, M BECKERS et al. Sputter deposition from a Ti2AlC target: process characterization and conditions for growth of Ti2AlC. Thin Solid Films, 518, 1621-1626(2010).

    [18] X WANG, Y ZHOU. High-temperature oxidation behavior of Ti2AlC in air. Oxidation of Metals, 59, 303-320(2003).

    [19] J ZHU, G QI, F WANG et al. Effect of aluminum content on synthesis of Ti2AlC and Ti3AlC2 during treatment in a high-energy mill and hot pressing. Metal Science and Heat Treatment, 53, 45-48(2011).

    [20] Z WANG, J SUN, B XU et al. Reducing the self-healing temperature of Ti2AlC MAX phase coating by substituting Al with Sn. Journal of the European Ceramic Society, 40, 197-201(2020).

    [21] J LIN Z, J ZHUO M, C ZHOU Y et al. Microstructural characterization of layered ternary Ti2AlC. Acta Materialia, 54, 1009-1015(2006).

    [22] E PAWEL R. The kinetics of oxidation of Zircaloy-4 in steam at high temperatures. Journal of The Electrochemical Society, 126, 1105(1979).

    [23] C WAGNER. Theoretical analysis of the diffusion processes determining the oxidation rate of alloys. Journal of The Electrochemical Society, 99, 369(1952).

    [24] H PARK J, G KIM H, Y PARK J et al. High temperature steam-oxidation behavior of arc ion plated Cr coatings for accident tolerant fuel claddings. Surface and Coatings Technology, 280, 256-259(2015).

    [25] A PINT B, A TERRANI K, P BRADY M et al. High temperature oxidation of fuel cladding candidate materials in steam-hydrogen environments. Journal of Nuclear Materials, 440, 420-427(2013).

    [26] A TERRANI K, A PINT B, M PARISH C et al. Silicon carbide oxidation in steam up to 2 MPa. Journal of the American Ceramic Society, 97, 2331-2352(2014).

    [27] S BASU, N OBANDO, A GOWDY et al. Long-term oxidation of Ti2AlC in air and water vapor at 1000-1300 ℃ temperature range. Journal of The Electrochemical Society, 159, C90-C96(2011).

    [28] I YOUNKER, M FRATONI. Neutronic evaluation of coating and cladding materials for accident tolerant fuels. Progress in Nuclear Energy, 88, 10-18(2016).

    Yiming LEI, Jie ZHANG, Guanghai BAI, Yanwei ZHANG, Xiaohui WANG, Jingyang WANG. Influence of Al Content on Oxidation Resistance of Phase-pure Ti2AlC under Simulated Loss-of-coolant Accident Conditions [J]. Journal of Inorganic Materials, 2021, 36(10): 1097