[1] Y IMANAKA. Multilayered Low Temperature Cofired Ceramics (LTCC) Technology, 1(2005).
[2] Y H WANG, J ZHOU, X M CUI et al. Development of low temperature cofired ceramic technology in material field. Journal of Inorganic Materials, 267(2006).
[3] Z Y WANG. Reliability analysis of mixed conductor LTCC substrate. Electronic Components & Materials, 7(2003).
[4] X Y CHEN, S X JIA, Y L WANG et al. Research on the process of LTCC substrates based on ENEPIG. Printed Circuit Information, 52(2021).
[5] A BEIKMOHAMADI, S STEWART, J PARISI et al. Electroplating and electroless plating process development for DuPont™ GreenTape™ 9K7 LTCC. Additional Papers and Presentations, 00283(2013).
[6] Y L WANG, J LI. The technology of Enepig of low temperature Co- fired ceramic substitute. Printed Circuit Information, 49(2020).
[7] K M NAIR, M A SKURSKI, J D VOULTOS. Nickel-gold Plateable Thick Film Silver Paste: US8609256B2.
[8] S THOMAS, P BALAKRISHNAN, M S SREEKALA. Fundamental Biomaterials:Ceramics, 250(2018).
[9] S M LEE, W B LIM, Y S CHO. Corrosion behavior of highly- crystallizable BaO-Nd2O3-TiO2-B2O3 glass-based composites. Corrosion Science, 399(2013).
[10] W B LIM, D W SHIN, B C MOHANTY et al. Chemical durability of anorthite-based low temperature co-fired ceramics. Journal of the Ceramic Society of Japan, 1138(2009).
[11] Y H JO, M S KANG, K W CHUNG et al. Chemical stability and dielectric properties of RO-La2O3-B2O3 (R= Ca, Mg, Zn)-based ceramics. Materials Research Bulletin, 361(2008).
[12] F STEINHÄUßER, A TALAI, G GÖLTL et al. Concentration and temperature dependent selectivity of the LTCC porosification process with phosphoric acid. Ceramics International, 714(2017).
[13] J KANG, J WANG, X ZHOU et al. Effects of alkali metal oxides on crystallization behavior and acid corrosion resistance of cordierite-based glass-ceramics. Journal of Non-Crystalline Solids, 184(2018).
[14] A HAJIAN, M STÖGER-POLLACH, M SCHNEIDER et al. Porosification behaviour of LTCC substrates with potassium hydroxide. Journal of the European Ceramic Society, 2369(2018).
[15] S N SALAMA, S M SALMAN. Characterization of glass-ceramic corrosion and durability. Journal of the European Ceramic Society, 521(1994).
[16] S GHOSH, S DATTA. Surface degradation behaviour of MgO- Al2O3-TiO2-SiO2 based glass-ceramics. Transactions of the Indian Ceramic Society, 216(2014).
[17] M T SEBASTIAN, H JANTUNEN. Low loss dielectric materials for LTCC applications: a review. International Materials Reviews, 57(2008).
[18] T WANG, Y WANG, H YANG et al. Structure, dielectric properties of low-temperature-sintering BaTiO3-based glass-ceramics for energy storage. Journal of Advanced Dielectrics, 1850(2018).
[19] L ĆURKOVIĆ, M F JELAČA, S KURAJICA. Corrosion behavior of alumina ceramics in aqueous HCl and H2SO4solutions. Corrosion Science, 872(2008).
[20] D E CLARK, B K ZOITOS. Corrosion of Glass, Ceramics and Ceramic Superconductor: Principles, Testing, Characterization and Applications. New Jersey: Noyes Publications, 2(1992).
[21] J G SPEIGHT. Lange's Handbook of Chemistry, 237(2005).
[22] A A OSIPOV, L M OSIPOVA. Structural studies of Na2O-B2O3 glasses and melts using high-temperature Raman spectroscopy. Physica B: Condensed Matter, 4718(2010).
[23] S V STEFANOVSKY, K M FOX, J C MARRA. Infrared and raman spectroscopic study of glasses in the Al2O3-B2O3-Fe2O3- Na2O-SiO2 system. MRS Online Proceedings Library (OPL), 53(2013).
[26] C D YIN, M OKUNO, H MORIKAWA et al. Structural analysis of CaSiO3 glass by X-ray diffraction and Raman spectroscopy. Journal of Non-crystalline Solids, 167(1986).
[27] Z WANG, Q SHU, K CHOU. Structure of CaO-B2O3-SiO2-TiO2 glasses: a Raman spectral study. ISIJ International, 1021(2011).
[28] D R NEUVILLE, LIGNY D DE, G S HENDERSON. Advances in Raman spectroscopy applied to earth and material sciences. Reviews in Mineralogy and Geochemistry, 509(2014).
[29] S GIN, A ABDELOUAS, L J CRISCENTI et al. An international initiative on long-term behavior of high-level nuclear waste glass. Materials Today, 243(2013).
[30] G S FRANKEL, J D VIENNA, J LIAN et al. A comparative review of the aqueous corrosion of glasses, crystalline ceramics, and metals. npj Materials Degradation, 15(2018).
[31] G S FRANKEL, J D VIENNA, J LIAN et al. Recent advances in corrosion science applicable to disposal of high-level nuclear waste. Chemical Reviews, 12327(2021).
[32] R A RAHIMI, S K SADRNEZHAAD, G RAISALI. Chemical durability of lead silicate glass in HNO3, HCl and H2SO4 aqueous acid solutions. Journal of Non-crystalline Solids, 169(2009).
[33] G D SALDI, S J KÖHLER, N MARTY et al. Dissolution rates of talc as a function of solution composition, pH and temperature. Geochimica et Cosmochimica Acta, 3446(2007).
[34] J WANG. Thermodynamic equilibrium and kinetic fundamentals of oxide dissolution in aqueous solution. Journal of Materials Research, 898(2020).
[35] G H CARTLEDGE. Studies on the periodic system. I. The ionic potential as a periodic function. Journal of the American Chemical Society, 2855(1928).
[36] G H CARTLEDGE. Studies on the periodic system. II. The ionic potential and related properties. Journal of the American Chemical Society, 2863(1928).
[37] B C BUNKER. Molecular mechanisms for corrosion of silica and silicate glasses. Journal of Non-Crystalline Solids, 300(1994).
[38] M COLLIN, M FOURNIER, P FRUGIER et al. Structure of international simple glass and properties of passivating layer formed in circumneutral pH conditions. npj Materials Degradation, 4(2018).
[39] E H OELKERS, J SCHOTT. An experimental study of enstatite dissolution rates as a function of pH, temperature, and aqueous Mg and Si concentration, and the mechanism of pyroxene/pyroxenoid dissolution. Geochimica et Cosmochimica Acta, 1219(2001).
[40] S GIN, L NEILL, M FOURNIER et al. The controversial role of inter-diffusion in glass alteration. Chemical Geology, 115(2016).
[41] J SCHOTT, O S POKROVSKY, O SPALLA et al. Formation, growth and transformation of leached layers during silicate minerals dissolution: the example of wollastonite. Geochimica et Cosmochimica Acta, 259(2012).
[42] P ZAPOL, H HE, K D KWON et al. First-principles study of hydrolysis reaction barriers in a sodium borosilicate glass. International Journal of Applied Glass Science, 395(2013).
[43] S L BRANTLEY. Kinetics of Water-rock Interaction, 151(2008).
[44] C CAILLETEAU, F ANGELI, F DEVREUX et al. Insight into silicate- glass corrosion mechanisms. Nature Materials, 978(2008).